XH55BMTΦK/Ю-BД Stainless Steels

XH55BMTΦK/Ю-BД - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH55BMTΦK/Ю-BД grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 0.45
Mn - 0.35
P - -
S - -
Cr 9.00 12.00
Ni - remaining
Mo 4.00 6.00
Al 3.60 4.50
Ti 1.40 2.00
Fe - 5.00
Co 12.00 15.50
W 4.50 6.00
V 0.20 0.80
B - 0.020

XH55BMTΦK/Ю-BД - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH55BMTΦK/Ю-BД

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
633 (≥) 954 (≥) 11 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade XH55BMTΦK/Ю-BД

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
954 (≥) 223 (≥) 21 21 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
522 295 155

Equivalent Products

We can customize the production of XH55BMTΦK/Ю-BД grade, contact us for the best solution.
sales@specificsteel.com