XH55BMTKЮ Special Alloy

Chemical composition%of the ladle analysis of gradeXH55BMTKЮ

C(%)Si(%)Mn(%)Cr(%)Ni(%)Mo(%)V(%)W(%)Co(%)B(%)Al(%)Ti(%)
0.04-0.10Max 0.50Max 0.509.0-12.0Balance4.00-6.000.20-0.804.50-6.5012.0-16.0Max 0.023.60-4.501.40-2.00
XH55BMTKЮ

Mechanical properties of gradeXH55BMTKЮ

Proof strength
Rp0.2(MPa)
Tensile strength
Rm(MPa)
Impact energy
KV(J)
Elongation at fracture
A(%)
Reduction in cross section on fracture
Z(%)
As-Heat-Treated Condition Brinell hardness(HBW)
959(≥) 614(≥) 42 21 13 Solution and Aging,Annealing,Ausaging,Q+T,etc 422

Physical properties of grade XH55BMTKЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J/kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
299(≥) 477(≥) 32 33 12 Solution and Aging,Annealing,Ausaging,Q+T,etc 443
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0)N/mm2
Creep rupture strength
(10000h)
(Rp1,0)N/mm2
931 599 257

XH55BMTKЮ Range of products

Product type Products Dimension Processes Deliver Status
Plates/Sheets Plates/Sheets 0.08-200mm(T)*W*L Forging,hot rolling and cold rolling Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Steel Bar Round Bar,Flat Bar,Square Bar Φ8-1200mm*L Forging,hot rolling and cold rolling,Cast Black,Rough Turning,Shot Blasting,
Coil/Strip Steel Coil/Steel Strip 0.03-16.0x1200mm Cold-Rolled&Hot-Rolled Annealed,Solution and Aging,Q+T,ACID-WASHED,Shot Blasting
Pipes/Tubes Seamless Pipes/Tubes,Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion,Cold Drawn,Welded Annealed,Solution and Aging,Q+T,ACID-WASHED

Equivalent Grade