XH56BMKЮ Stainless Steels

XH56BMKЮ - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH56BMKЮ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.60
Mn - 0.30
P - 0.015
S - 0.010
Cr 8.50 10.50
Ni - remaining
Mo 6.50 8.00
Al 5.40 6.20
Ti - -
Fe - 1.50
Co 12.00 16.00
W 6.00 7.50
Ce - 0.02
B - 0.020

XH56BMKЮ - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH56BMKЮ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
399 (≥) 264 (≥) 21 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade XH56BMKЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
121 (≥) 576 (≥) 24 22 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
117 931 151

Equivalent Grade

Equivalent Products

We can customize the production of XH56BMKЮ grade, contact us for the best solution.