XH62MBKЮ Stainless Steels

XH62MBKЮ - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH62MBKЮ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.60
Mn - 0.30
P - 0.015
S - 0.010
Cr 8.50 10.50
Ni - remaining
Mo 9.00 11.50
Al 4.20 4.90
Ti - -
Fe - 4.00
W 4.30 6.00
Co 4.00 6.00
B - 0.02
Ce - 0.02

XH62MBKЮ - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH62MBKЮ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
421 (≥) 281 (≥) 32 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade XH62MBKЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
248 (≥) 429 (≥) 21 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
241 511 574

Equivalent Products

We can customize the production of XH62MBKЮ grade, contact us for the best solution.