XH65BMTЮ Stainless Steels

XH65BMTЮ - Specification & Application

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Chemical composition(wt.%) of XH65BMTЮ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.60
Mn - 0.50
P - 0.015
S - 0.012
Cr 15.00 17.00
Ni - remaining
Mo 3.50 4.50
Al 1.20 1.60
Ti 1.20 1.60
Fe - 3.00
W 8.50 10.00
B - 0.010
Ce - 0.025

XH65BMTЮ - Detail

Russia GOCT standard deformation of high temperature alloy grades and chemical composition

Mechanical properties of grade XH65BMTЮ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
431 (≥) 853 (≥) 33 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade XH65BMTЮ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
321 (≥) 343 (≥) 32 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 331
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
934 871 193

Equivalent Grade

Equivalent Products

We can customize the production of XH65BMTЮ grade, contact us for the best solution.