A 240 N08800 Stainless Steels to A 240/A 240M (2013)

A 240 N08800 - Specification & Application

  • A 240/A 240M (2013) - Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of A 240 N08800 grade: to A 240/A 240M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 1.50
Si - 1.00
P - 0.045
S - 0.015
Cr 19.00 23.00
Ni 30.00 35.00
Mo - -
Ti 0.15 0.60
Al 0.15 0.60

A 240 N08800 - Detail

Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade A 240 N08800 A 240/A 240M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
986 (≥) 292 (≥) 14 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade A 240 N08800 A 240/A 240M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
122 (≥) 454 (≥) 33 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
399 488 911

Equivalent Products

We can customize the production of A 240 N08800 grade, contact us for the best solution.