A 479 S31254 Stainless Steels to A 479/A 479M (2013)

A 479 S31254 - Specification & Application

  • A 479/A 479M (2013) - Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Chemical composition(wt.%) of A 479 S31254 grade: to A 479/A 479M (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.02
Mn - 1.00
Si - 0.80
P - 0.03
S - 0.01
Cr 19.50 20.50
Ni 17.50 18.50
Mo 6.00 6.50
Cu 0.50 1.00
N 0.18 0.22

A 479 S31254 - Detail

Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Mechanical properties of grade A 479 S31254 A 479/A 479M (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
926 (≥) 779 (≥) 32 13 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 233

Physical properties of grade A 479 S31254 A 479/A 479M (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
767 (≥) 723 (≥) 22 44 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
389 325 192

Equivalent Products

We can customize the production of A 479 S31254 grade, contact us for the best solution.