B 163 N08800 Stainless Steels to B 163 (2011)

B 163 N08800 - Specification & Application

  • B 163 (2011) - Standard Specification for Seamless Nickel and Nickel Alloy (UNS N06845) Condenser and Heat-Exchanger Tubes

Standard Specification for Seamless Nickel and Nickel Alloy (UNS N06845) Condenser and Heat-Exchanger Tubes

Chemical composition(wt.%) of B 163 N08800 grade: to B 163 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 1.50
Si - 1.00
P - 0.045
S - 0.015
Cr 19.00 23.00
Ni 30.00 35.00
Mo - -
Ti 0.15 0.60
Al 0.15 0.60

B 163 N08800 - Detail

Standard Specification for Seamless Nickel and Nickel Alloy (UNS N06845) Condenser and Heat-Exchanger Tubes

Mechanical properties of grade B 163 N08800 B 163 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
672 (≥) 349 (≥) 21 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade B 163 N08800 B 163 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
816 (≥) 543 (≥) 12 33 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
119 291 167

Equivalent Products

We can customize the production of B 163 N08800 grade, contact us for the best solution.
sales@specificsteel.com