ER 209 Stainless Steels to A5.9/A5.9M

ER 209 - Specification & Application

  • A5.9/A5.9M - Bare Stainless Steel Welding Electrodes and Rods

Bare Stainless Steel Welding Electrodes and Rods

Chemical composition(wt.%) of ER 209 grade: to A5.9/A5.9M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.30
Mn - 0.80
Cr - 19.00
Ni - 14.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining
Nb - 1.60

ER 209 - Detail

Bare Stainless Steel Welding Electrodes and Rods

Mechanical properties of grade ER 209 A5.9/A5.9M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
481 (≥) 712 (≥) 14 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade ER 209 A5.9/A5.9M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
471 (≥) 156 (≥) 34 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 243
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
973 249 429

Equivalent Products

We can customize the production of ER 209 grade, contact us for the best solution.
sales@specificsteel.com