ER 316H Stainless Steels to SFA-5.9/SFA-5.9M

ER 316H - Specification & Application

  • SFA-5.9/SFA-5.9M - Bare Stainless Steel Welding Electrodes and Rods

Bare Stainless Steel Welding Electrodes and Rods

Chemical composition(wt.%) of ER 316H grade: to SFA-5.9/SFA-5.9M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.10
Si - 1.00
Mn - 2.00
P - 0.04
S - 0.03
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00

ER 316H - Detail

Bare Stainless Steel Welding Electrodes and Rods

Mechanical properties of grade ER 316H SFA-5.9/SFA-5.9M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
691 (≥) 812 (≥) 33 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade ER 316H SFA-5.9/SFA-5.9M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
271 (≥) 436 (≥) 12 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
455 233 534

Equivalent Products

We can customize the production of ER 316H grade, contact us for the best solution.