03X13AΓ19 Stainless Steels

03X13AΓ19 - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 03X13AΓ19 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.60
Mn 19.00 22.00
P - 0.035
S - 0.025
Cr 12.00 15.00
Ni - 1.00
Mo - 0.30
N 0.05 0.10
Ca - 0.10
V - 0.10
Ce - 0.10

03X13AΓ19 - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 03X13AΓ19

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
439 (≥) 879 (≥) 24 34 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 411

Physical properties of grade 03X13AΓ19

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
949 (≥) 177 (≥) 11 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
437 429 663

Equivalent Grade

Equivalent Products

We can customize the production of 03X13AΓ19 grade, contact us for the best solution.