06X17Γ15AБ Stainless Steels

06X17Γ15AБ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 06X17Γ15AБ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.60
Mn 14.50 16.50
P - 0.045
S - 0.035
Cr 16.30 18.30
Ni - 0.60
Mo - 0.30
B 0.0030 0.0080
Nb 0.35 0.90
Co - 0.20
N - 0.04
Al - 0.05
V - 0.15

06X17Γ15AБ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 06X17Γ15AБ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
356 (≥) 768 (≥) 41 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade 06X17Γ15AБ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
981 (≥) 578 (≥) 24 41 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
522 336 737

Equivalent Grade

Equivalent Products

We can customize the production of 06X17Γ15AБ grade, contact us for the best solution.