17-7PH Stainless Steels to SAE AMS 5528H (2007)

17-7PH - Specification & Application

  • SAE AMS 5528H (2007) - Steel, Corrosion-Resistant, Sheet, Strip, and Plate 17Cr - 7.1Ni - 1.1Al Solution Heat Treated, Precipitation Hardenable
  • SAE AMS 5529J (2012) - Steel, Corrosion Resistant, Sheet and Strip 17Cr - 7.1Ni - 1.1Al Solution Heat Treated and Cold Rolled, Precipitation Hardenable 0.0015 to 0.050 Inch (0.038 to 1.27 mm) Nominal Thickness
  • SAE AMS 5568G (2011) - Steel, Corrosion and Heat Resistant, Welded Tubing 17Cr - 7.1Ni - 1.1Al Solution Heat Treated, Precipitation-Hardenable
  • SAE AMS 5644D (1964) - Steel Bars and Forgings, Corrosion Heat Resistant 17Cr - 7Ni - 1Al
  • SAE AMS 5678F (2007) - Steel, Corrosion Resistant, Wire 17Cr - 7.1Ni - 1.1Al Cold Drawn, Precipitation-Hardenable
  • SAE J 217 (1994) - Stainless steel 17-7 PH spring wire and springs
  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Steel, Corrosion-Resistant, Sheet, Strip, and Plate 17Cr - 7.1Ni - 1.1Al Solution Heat Treated, Precipitation Hardenable

Chemical composition(wt.%) of 17-7PH grade: to SAE AMS 5528H (2007)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.09
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.040
Ni 6.50 7.75
Cr 16.00 18.00
Al 0.75 1.50

17-7PH - Detail

Steel, Corrosion-Resistant, Sheet, Strip, and Plate 17Cr - 7.1Ni - 1.1Al Solution Heat Treated, Precipitation Hardenable 

Mechanical properties of grade 17-7PH SAE AMS 5528H (2007)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
799 (≥) 656 (≥) 13 23 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 442

Physical properties of grade 17-7PH SAE AMS 5528H (2007)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
968 (≥) 968 (≥) 13 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
373 439 322