A 29 41L18 Stainless Steels to A 29/A 29M (2012)

A 29 41L18 - Specification & Application

  • A 29/A 29M (2012) - Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Chemical composition(wt.%) of A 29 41L18 grade: to A 29/A 29M (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.20
Mn - 0.30
P - -
S - -
Ni - 0.15
Cr 28.00 30.00
Al - -
Cu - 0.15
Ti - -
Fe - -
N - 0.02
Mo 3.50 4.20

A 29 41L18 - Detail

Steel Bars, Carbon and Alloy, Hot-Wrought, General Requirements for

Mechanical properties of grade A 29 41L18 A 29/A 29M (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
573 (≥) 166 (≥) 24 22 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade A 29 41L18 A 29/A 29M (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
149 (≥) 545 (≥) 24 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 342
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
538 648 343

Equivalent Products

We can customize the production of A 29 41L18 grade, contact us for the best solution.