A 322 61L18 Stainless Steels to A 322 (2013)

A 322 61L18 - Specification & Application

  • A 322 (2013) - Steel Bars, Alloy, Standard Grades

Steel Bars, Alloy, Standard Grades

Chemical composition(wt.%) of A 322 61L18 grade: to A 322 (2013)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.75
Mn - 0.75
P - -
S - -
Ni - 0.50
Cr 25.00 27.00
Al - -
Cu - 0.20
Ti - -
Fe - -
N - 0.04
Mo 0.75 1.50

A 322 61L18 - Detail

Steel Bars, Alloy, Standard Grades

Mechanical properties of grade A 322 61L18 A 322 (2013)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
434 (≥) 821 (≥) 11 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 414

Physical properties of grade A 322 61L18 A 322 (2013)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
448 (≥) 463 (≥) 12 13 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 434
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
486 619 897

Equivalent Products

We can customize the production of A 322 61L18 grade, contact us for the best solution.
sales@specificsteel.com