A 541 Class 8 Stainless Steels to A 541/A 541M (2010)

A 541 Class 8 - Specification & Application

  • A 541/A 541M (2010) - Quenched and Tempered Carbon and Alloy Steel Forgings for Pressure Vessel Components

Quenched and Tempered Carbon and Alloy Steel Forgings for Pressure Vessel Components

Chemical composition(wt.%) of A 541 Class 8 grade: to A 541/A 541M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 0.50
Mn - 1.00
P - -
S - -
Ni - -
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - -
W - 3.00

A 541 Class 8 - Detail

Quenched and Tempered Carbon and Alloy Steel Forgings for Pressure Vessel Components

Mechanical properties of grade A 541 Class 8 A 541/A 541M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
393 (≥) 493 (≥) 11 24 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade A 541 Class 8 A 541/A 541M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
351 (≥) 683 (≥) 42 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
429 232 141

Equivalent Products

We can customize the production of A 541 Class 8 grade, contact us for the best solution.