A 632 S34800 Stainless Steels to A 632 (2009)

A 632 S34800 - Specification & Application

  • A 632 (2009) - Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service

Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service

Chemical composition(wt.%) of A 632 S34800 grade: to A 632 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 9.00 11.30
Ta - 0.10
Co - 0.20

A 632 S34800 - Detail

Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service

Mechanical properties of grade A 632 S34800 A 632 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
148 (≥) 722 (≥) 11 21 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade A 632 S34800 A 632 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
946 (≥) 649 (≥) 31 24 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
192 218 846