A 752 Grade 6118 Stainless Steels to A 752M (2010)

A 752 Grade 6118 - Specification & Application

  • A 752M (2010) - General Requirements for Wire Rods and Coarse Round Wire, Alloy Steel [Metric]

General Requirements for Wire Rods and Coarse Round Wire, Alloy Steel [Metric]

Chemical composition(wt.%) of A 752 Grade 6118 grade: to A 752M (2010)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.75
Mn - 0.75
P - -
S - -
Ni - 0.50
Cr 25.00 27.00
Al - -
Cu - 0.20
Ti - -
Fe - -
N - 0.04
Mo 0.75 1.50

A 752 Grade 6118 - Detail

General Requirements for Wire Rods and Coarse Round Wire, Alloy Steel [Metric]

Mechanical properties of grade A 752 Grade 6118 A 752M (2010)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
241 (≥) 218 (≥) 11 41 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade A 752 Grade 6118 A 752M (2010)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
392 (≥) 591 (≥) 24 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
833 478 756

Equivalent Products

We can customize the production of A 752 Grade 6118 grade, contact us for the best solution.