B 435 N06002 Stainless Steels to B 435 (2011)

B 435 N06002 - Specification & Application

  • B 435 (2011) - UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip

UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip

Chemical composition(wt.%) of B 435 N06002 grade: to B 435 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.05
Mn - 1.50
P - 0.04
S - 0.01
Ni - remaining
Cr 0.50 1.50
Al 0.10 0.50
Cu - 0.50
Ti - -
Fe 1.00 6.00
Mo 26.00 30.00
Co - 2.50

B 435 N06002 - Detail

UNS N06002, UNS N06230, UNS N12160, and UNS R30556 Plate, Sheet, and Strip

Mechanical properties of grade B 435 N06002 B 435 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
669 (≥) 366 (≥) 12 13 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade B 435 N06002 B 435 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
398 (≥) 521 (≥) 41 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
272 822 252

Equivalent Products

We can customize the production of B 435 N06002 grade, contact us for the best solution.