Nickel-Chromium-Molybdenum-Columbium Alloys (UNS N06625 and UNS N06852) and Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219) Pipe and Tube
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.01 | ||
Si | - | 0.05 | ||
Mn | - | 1.50 | ||
P | - | 0.04 | ||
S | - | 0.01 | ||
Ni | - | remaining | ||
Cr | 0.50 | 1.50 | ||
Al | 0.10 | 0.50 | ||
Cu | - | 0.50 | ||
Ti | - | - | ||
Fe | 1.00 | 6.00 | ||
Mo | 26.00 | 30.00 | ||
Co | - | 2.50 |
Nickel-Chromium-Molybdenum-Columbium Alloys (UNS N06625 and UNS N06852) and Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219) Pipe and Tube
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
133 (≥) | 626 (≥) | 22 | 24 | 34 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 334 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
575 (≥) | 474 (≥) | 23 | 32 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 413 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
156 | 854 | 654 |
We can customize the production of B 444 N06219 grade, contact us for the best solution.