B 446 N06650 Stainless Steels to B 446 (2008)

B 446 N06650 - Specification & Application

  • B 446 (2008) - Nickel-Chromium-Molybdenum-Columbium Alloy (UNS N06625), Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219), and Nickel-Chromium-Molybdenum-Tungsten Alloy (UNS N06650) Rod and Bar

Nickel-Chromium-Molybdenum-Columbium Alloy (UNS N06625), Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219), and Nickel-Chromium-Molybdenum-Tungsten Alloy (UNS N06650) Rod and Bar

Chemical composition(wt.%) of B 446 N06650 grade: to B 446 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.05
Mn - 1.50
P - 0.04
S - 0.01
Ni - remaining
Cr 0.50 1.50
Al 0.10 0.50
Cu - 0.50
Ti - -
Fe 1.00 6.00
Mo 26.00 30.00
Co - 2.50

B 446 N06650 - Detail

Nickel-Chromium-Molybdenum-Columbium Alloy (UNS N06625), Nickel-Chromium-Molybdenum-Silicon Alloy (UNS N06219), and Nickel-Chromium-Molybdenum-Tungsten Alloy (UNS N06650) Rod and Bar

Mechanical properties of grade B 446 N06650 B 446 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
499 (≥) 444 (≥) 43 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 223

Physical properties of grade B 446 N06650 B 446 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
757 (≥) 922 (≥) 12 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 411
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
215 761 367

Equivalent Products

We can customize the production of B 446 N06650 grade, contact us for the best solution.