B 512 N08330 Stainless Steels to B 512 (2009)

B 512 N08330 - Specification & Application

  • B 512 (2009) - Nickel-Chromium-Silicon Alloy (UNS N08330) Billets and Bars

Nickel-Chromium-Silicon Alloy (UNS N08330) Billets and Bars

Chemical composition(wt.%) of B 512 N08330 grade: to B 512 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 2.00
Si - 1.50
P - 0.045
S - 0.04
Cr 14.00 17.00
Ni 33.00 37.00

B 512 N08330 - Detail

Nickel-Chromium-Silicon Alloy (UNS N08330) Billets and Bars

Mechanical properties of grade B 512 N08330 B 512 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
921 (≥) 917 (≥) 13 23 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade B 512 N08330 B 512 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
994 (≥) 842 (≥) 34 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
811 942 984