F1058 Grade 2 Stainless Steels to F1058 (2008)

F1058 Grade 2 - Specification & Application

  • F1058 (2008) - Standard Specification for Wrought 40Cobalt-20Chromium-16Iron-15Nickel-7Molybdenum Alloy Wire and Strip for Surgical Implant Applications (UNS R30003 and UNS R30008)

Standard Specification for Wrought 40Cobalt-20Chromium-16Iron-15Nickel-7Molybdenum Alloy Wire and Strip for Surgical Implant Applications (UNS R30003 and UNS R30008)

Chemical composition(wt.%) of F1058 Grade 2 grade: to F1058 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.20
Si 1.00 1.40
Mn 0.50 0.80
P - -
S - -
Ni 19.00 22.00
Cr 7.00 9.00
Al - -
Cu - -
Ti - -
Fe - -
Mo - -
Co - -

F1058 Grade 2 - Detail

Standard Specification for Wrought 40Cobalt-20Chromium-16Iron-15Nickel-7Molybdenum Alloy Wire and Strip for Surgical Implant Applications (UNS R30003 and UNS R30008)

Mechanical properties of grade F1058 Grade 2 F1058 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
247 (≥) 258 (≥) 21 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade F1058 Grade 2 F1058 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
284 (≥) 248 (≥) 22 14 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
858 966 359

Equivalent Products

We can customize the production of F1058 Grade 2 grade, contact us for the best solution.