H11 Tool Die Steels

H11 - Specification & Application

Hot-Work Tool Steel

Chemical composition(wt.%) of H11 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.33 0.43
Si 0.80 1.20
Mn 0.20 0.50
P - 0.030
S - 0.030
Cr 4.75 5.50
Mo 1.10 1.60
V 0.30 0.60
W - -
Ni+Cu - 0.75

H11 - Detail

Hot-Work Tool Steel

Mechanical properties of grade H11

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
679 (≥) 331 (≥) 43 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade H11

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
243 (≥) 151 (≥) 44 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 212
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
518 868 556
We can customize the production of H11 grade, contact us for the best solution.