HARPER 200 Stainless Steels to SAE J 470 (1976)

HARPER 200 - Specification & Application

  • SAE J 470 (1976) - Wrought nickel and nickel-related alloys

Wrought nickel and nickel-related alloys

Chemical composition(wt.%) of HARPER 200 grade: to SAE J 470 (1976)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.30
Mn - 0.80
Cr - 19.00
Ni - 14.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining
Nb - 1.60

HARPER 200 - Detail

Wrought nickel and nickel-related alloys

Mechanical properties of grade HARPER 200 SAE J 470 (1976)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
955 (≥) 192 (≥) 43 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade HARPER 200 SAE J 470 (1976)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
895 (≥) 988 (≥) 13 22 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
774 179 243