J92999 Stainless Steels

J92999 - Specification & Application

Cast Chromium Nickel Molybdenum Stainless Steel

Chemical composition(wt.%) of J92999 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.08 0.15
Si - 0.75
Mn 1.00 2.00
P - -
S - 0.03
Ni 8.50 10.50
Cr 27.00 31.00
Al - -
Cu - 0.50
Ti - -
Fe - -
N - -
Mo - 0.50

J92999 - Detail

Cast Chromium Nickel Molybdenum Stainless Steel

Mechanical properties of grade J92999

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
559 (≥) 482 (≥) 32 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade J92999

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
558 (≥) 129 (≥) 42 32 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 241
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
341 123 574

Equivalent Products