K30736 Stainless Steels

K30736 - Specification & Application

Alloy Steel Electrode (A213)

Chemical composition(wt.%) of K30736 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn 3.75 4.75
P - 0.045
S - 0.03
Ni 9.00 10.50
Cr 19.00 22.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo - -
V - -

K30736 - Detail

Alloy Steel Electrode (A213)

Mechanical properties of grade K30736

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
655 (≥) 611 (≥) 43 11 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade K30736

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
525 (≥) 845 (≥) 23 42 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
567 582 733
We can customize the production of K30736 grade, contact us for the best solution.