S30600 Stainless Steels

S30600 - Specification & Application

Stainless steel and heat resistant steel

Chemical composition(wt.%) of S30600 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.018
Si 3.70 4.30
Mn - 2.00
P - 0.02
S - 0.02
Cr 17.0 18.5
Ni 14.0 15.5
Mo - 0.20
Cu - 0.50

S30600 - Detail

Stainless steel and heat resistant steel

Mechanical properties of grade S30600

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
761 (≥) 582 (≥) 24 14 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade S30600

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
343 (≥) 855 (≥) 12 34 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
468 689 457

Equivalent Products

We can customize the production of S30600 grade, contact us for the best solution.