S30880 Stainless Steels

S30880 - Specification & Application

Austenitic Chromium Nickel Stainless Steel Bare Filler Metal

Chemical composition(wt.%) of S30880 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 0.25 0.60
Mn 1.00 2.50
P - 0.03
S - 0.03
Cr 19.5 22.0
Ni 9.00 11.0

S30880 - Detail

Austenitic Chromium Nickel Stainless Steel Bare Filler Metal

Mechanical properties of grade S30880

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
594 (≥) 389 (≥) 22 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade S30880

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
318 (≥) 212 (≥) 22 43 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
619 145 792