S34720 Stainless Steels

S34720 - Specification & Application

Austenitic Chromium Nickel Free-Machining Stainless Steel (Columbium stabilized)

Chemical composition(wt.%) of S34720 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si - 1.00
P - 0.04
S 0.18 0.35
Cr 17.00 19.00
Ni 9.00 12.00

S34720 - Detail

Austenitic Chromium Nickel Free-Machining Stainless Steel (Columbium stabilized)

Mechanical properties of grade S34720

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
718 (≥) 329 (≥) 22 31 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade S34720

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
467 (≥) 431 (≥) 21 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
141 875 932