SA-182 F 10 Stainless Steels to SA-182/SA-182M

SA-182 F 10 - Specification & Application

  • SA-182/SA-182M - Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Chemical composition(wt.%) of SA-182 F 10 grade: to SA-182/SA-182M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.10 0.20
Si 1.00 1.40
Mn 0.50 0.80
P - -
S - -
Ni 19.00 22.00
Cr 7.00 9.00
Al - -
Cu - -
Ti - -
Fe - -
Mo - -
Co - -

SA-182 F 10 - Detail

Specification for Forged or Rolled Alloy and Stainless Steel Pipe Flanges, Forged Fittings, and Valves and Parts for High-Temperature Service

Mechanical properties of grade SA-182 F 10 SA-182/SA-182M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
699 (≥) 546 (≥) 31 22 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade SA-182 F 10 SA-182/SA-182M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
313 (≥) 775 (≥) 12 41 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
969 777 618

Equivalent Products

We can customize the production of SA-182 F 10 grade, contact us for the best solution.