SA-213 TP317LMN Stainless Steels to SA-213/SA-213M

SA-213 TP317LMN - Specification & Application

  • SA-213/SA-213M - Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of SA-213 TP317LMN grade: to SA-213/SA-213M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.30
Si - 0.70
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 27.00
Cr 18.00 20.00
Al - -
Cu - 0.75
Ti - -
Fe - -
N - 0.10
Mo 4.00 5.00
V - 0.08

SA-213 TP317LMN - Detail

Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade SA-213 TP317LMN SA-213/SA-213M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
234 (≥) 241 (≥) 23 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade SA-213 TP317LMN SA-213/SA-213M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
147 (≥) 577 (≥) 14 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
473 257 737

Equivalent Products