SA-336 Grade F316LN Stainless Steels to SA-336/SA-336M

SA-336 Grade F316LN - Specification & Application

  • SA-336/SA-336M - Alloy Steel Forgings for Pressure and High-Temperature Parts

Alloy Steel Forgings for Pressure and High-Temperature Parts

Chemical composition(wt.%) of SA-336 Grade F316LN grade: to SA-336/SA-336M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N 0.10 0.16

SA-336 Grade F316LN - Detail

Alloy Steel Forgings for Pressure and High-Temperature Parts

Mechanical properties of grade SA-336 Grade F316LN SA-336/SA-336M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
564 (≥) 696 (≥) 12 33 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade SA-336 Grade F316LN SA-336/SA-336M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
548 (≥) 237 (≥) 12 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
435 475 574

Equivalent Products

We can customize the production of SA-336 Grade F316LN grade, contact us for the best solution.