SA-815 WPS32205 Stainless Steels to SA-815/SA-815M

SA-815 WPS32205 - Specification & Application

  • SA-815/SA-815M - Specification for Wrought Ferritic, Ferritic /Austenitic, and Martensitic Stainless Steel Piping Fittings

Specification for Wrought Ferritic, Ferritic /Austenitic, and Martensitic Stainless Steel Piping Fittings

Chemical composition(wt.%) of SA-815 WPS32205 grade: to SA-815/SA-815M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.02
Cr 22.00 23.00
Ni 4.50 6.50
Mo 3.00 3.50
N 0.14 0.20

SA-815 WPS32205 - Detail

Specification for Wrought Ferritic, Ferritic /Austenitic, and Martensitic Stainless Steel Piping Fittings

Mechanical properties of grade SA-815 WPS32205 SA-815/SA-815M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
232 (≥) 136 (≥) 42 13 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 143

Physical properties of grade SA-815 WPS32205 SA-815/SA-815M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
619 (≥) 942 (≥) 13 24 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
266 692 719

Equivalent Products

We can customize the production of SA-815 WPS32205 grade, contact us for the best solution.