2331 Stainless Steels to SS 142331

2331 - Specification & Application

  • SS 142331 - Stainless steel - SS steel 2331

Stainless steel - SS steel 2331

Chemical composition(wt.%) of 2331 grade: to SS 142331

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 1.50
Mn - 2.00
P - 0.045
S - 0.030
Cr 16.00 19.00
Ni 6.50 9.50
Mo - 0.80

2331 - Detail

Stainless steel - SS steel 2331

Mechanical properties of grade 2331 SS 142331

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
322 (≥) 299 (≥) 43 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade 2331 SS 142331

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
757 (≥) 367 (≥) 13 42 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
768 737 443

Equivalent Grade

Equivalent Products

We can customize the production of 2331 grade, contact us for the best solution.