SUS316LN Stainless Steels to SA/JIS G4303

SUS316LN - Specification & Application

  • SA/JIS G4303 - Specification for stainless steel bars

Specification for stainless steel bars

Chemical composition(wt.%) of SUS316LN grade: to SA/JIS G4303

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N 0.10 0.16

SUS316LN - Detail

Specification for stainless steel bars

Mechanical properties of grade SUS316LN SA/JIS G4303

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
351 (≥) 378 (≥) 21 42 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade SUS316LN SA/JIS G4303

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
733 (≥) 461 (≥) 41 11 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
531 426 798

Equivalent Products

We can customize the production of SUS316LN grade, contact us for the best solution.
sales@specificsteel.com