NiFe 25 Cr 20 NbTi Stainless Steels to SAE J 775 (2004)

NiFe 25 Cr 20 NbTi - Specification & Application

  • SAE J 775 (2004) - Engine poppet valve information report

Engine poppet valve information report

Chemical composition(wt.%) of NiFe 25 Cr 20 NbTi grade: to SAE J 775 (2004)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.30
Mn - 0.80
Cr - 19.00
Ni - 14.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining
Nb - 1.60

NiFe 25 Cr 20 NbTi - Detail

Engine poppet valve information report

Mechanical properties of grade NiFe 25 Cr 20 NbTi SAE J 775 (2004)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
118 (≥) 846 (≥) 43 43 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 114

Physical properties of grade NiFe 25 Cr 20 NbTi SAE J 775 (2004)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
796 (≥) 254 (≥) 44 23 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
318 634 371