R20033 Stainless Steels

R20033 - Specification & Application

Cr-Ni-Fe-Mo Austenitic stainless steel

Chemical composition(wt.%) of R20033 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.12
Si - 0.30
Mn - 0.80
Cr - 19.00
Ni - 14.00
Mo - -
Co - -
W - -
Al - -
Cu - -
Ti - -
Fe - remaining
Nb - 1.60

R20033 - Detail

Cr-Ni-Fe-Mo Austenitic stainless steel

Mechanical properties of grade R20033

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
712 (≥) 625 (≥) 32 23 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 232

Physical properties of grade R20033

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
713 (≥) 575 (≥) 44 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 311
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
979 448 855