S31803 Stainless Steels

S31803 - Specification & Application

Duplex (Austenitic-Ferritic) Chromium Nickel Molybdenum Nitrogen Stainless Steel

Chemical composition(wt.%) of S31803 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.03
S - 0.02
Cr 21.00 23.00
Ni 4.50 6.50
Mo 2.50 3.50
N 0.08 0.20

S31803 - Detail

Duplex (Austenitic-Ferritic) Chromium Nickel Molybdenum Nitrogen Stainless Steel

Mechanical properties of grade S31803

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
573 (≥) 497 (≥) 31 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade S31803

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
621 (≥) 724 (≥) 21 32 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 324
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
329 921 399

Equivalent Products

We can customize the production of S31803 grade, contact us for the best solution.