S32950 Stainless Steels

S32950 - Specification & Application

Duplex (Austenitic-Ferritic) Chromium Nickel Molybdenum Nitrogen Stainless Steel

Chemical composition(wt.%) of S32950 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 0.60
P - 0.035
S - 0.01
Cr 26.00 29.00
Ni 3.50 5.20
Mo 1.00 2.50
N 0.15 0.25

S32950 - Detail

Duplex (Austenitic-Ferritic) Chromium Nickel Molybdenum Nitrogen Stainless Steel

Mechanical properties of grade S32950

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
898 (≥) 614 (≥) 13 43 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade S32950

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
643 (≥) 131 (≥) 41 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
655 125 415

Equivalent Products

We can customize the production of S32950 grade, contact us for the best solution.