SA-213 S34565 Stainless Steels to SA-213/SA-213M

SA-213 S34565 - Specification & Application

  • SA-213/SA-213M - Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of SA-213 S34565 grade: to SA-213/SA-213M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn 5.00 7.00
Si - 1.00
P - 0.03
S - 0.01
Cr 23.00 25.00
Ni 16.00 18.00
Mo 4.00 5.00
N 0.40 0.60
Nb - 0.10

SA-213 S34565 - Detail

Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade SA-213 S34565 SA-213/SA-213M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
447 (≥) 252 (≥) 21 21 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade SA-213 S34565 SA-213/SA-213M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
759 (≥) 384 (≥) 42 22 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
459 631 757