SA-240 S32304 Stainless Steels to SA-240/SA-240M

SA-240 S32304 - Specification & Application

  • SA-240/SA-240M - Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Chemical composition(wt.%) of SA-240 S32304 grade: to SA-240/SA-240M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.50
Si - 1.00
P - 0.04
S - 0.04
Cr 21.50 24.50
Ni 3.00 5.50
Mo 0.05 0.60
N 0.05 0.20
Cu 0.05 0.60

SA-240 S32304 - Detail

Specification for Chromium and Chromium-Nickel Stainless Steel Plate, Sheet, and Strip for Pressure Vessels and for General Applications

Mechanical properties of grade SA-240 S32304 SA-240/SA-240M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
462 (≥) 997 (≥) 14 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade SA-240 S32304 SA-240/SA-240M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
883 (≥) 668 (≥) 43 22 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
862 995 555

Equivalent Products

We can customize the production of SA-240 S32304 grade, contact us for the best solution.