SA-249 S30815 Stainless Steels to SA-249/SA-249M

SA-249 S30815 - Specification & Application

  • SA-249/SA-249M - Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Chemical composition(wt.%) of SA-249 S30815 grade: to SA-249/SA-249M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.10
Mn - 0.80
Si 1.40 2.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 10.00 12.00
Mo - -
Al - 1.00
Ce 0.03 0.08

SA-249 S30815 - Detail

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Mechanical properties of grade SA-249 S30815 SA-249/SA-249M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
949 (≥) 926 (≥) 44 34 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 343

Physical properties of grade SA-249 S30815 SA-249/SA-249M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
874 (≥) 111 (≥) 23 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 111
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
862 113 847

Equivalent Products

We can customize the production of SA-249 S30815 grade, contact us for the best solution.