SA-358 N08367 Stainless Steels to SA-358/SA-358M

SA-358 N08367 - Specification & Application

  • SA-358/SA-358M - Electric-Fusion-Welded Austenitic Chromium-Nickel Alloy Steel Pipe for High-Temperature Service

Electric-Fusion-Welded Austenitic Chromium-Nickel Alloy Steel Pipe for High-Temperature Service

Chemical composition(wt.%) of SA-358 N08367 grade: to SA-358/SA-358M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.04
S - 0.03
Cr 20.00 22.00
Ni 23.50 25.50
Mo 6.00 7.00
N 0.18 0.25

SA-358 N08367 - Detail

Electric-Fusion-Welded Austenitic Chromium-Nickel Alloy Steel Pipe for High-Temperature Service

Mechanical properties of grade SA-358 N08367 SA-358/SA-358M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
533 (≥) 533 (≥) 44 33 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade SA-358 N08367 SA-358/SA-358M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
587 (≥) 455 (≥) 22 24 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 431
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
716 261 615
We can customize the production of SA-358 N08367 grade, contact us for the best solution.