SA-412 XM-11 Stainless Steels to SA-412

SA-412 XM-11 - Specification & Application

  • SA-412 - Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Plate, Sheet, and Strip

Stainless and Heat-Resisting Chromium-Nickel-Manganese Steel Plate, Sheet, and Strip

Chemical composition(wt.%) of SA-412 XM-11 grade: to SA-412

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Si - 1.00
Mn 8.00 10.0
P - 0.06
S - 0.03
Cr 19.0 21.5
Ni 5.50 7.50
N 0.15 0.40

SA-412 XM-11 - Detail

SA-412 XM-11

Mechanical properties of grade SA-412 XM-11 SA-412

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
934 (≥) 194 (≥) 14 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade SA-412 XM-11 SA-412

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
472 (≥) 591 (≥) 33 22 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 133
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
745 932 582

Equivalent Products

We can customize the production of SA-412 XM-11 grade, contact us for the best solution.