SA-479 S32550 Stainless Steels to SA-479/SA-479M

SA-479 S32550 - Specification & Application

  • SA-479/SA-479M - Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Chemical composition(wt.%) of SA-479 S32550 grade: to SA-479/SA-479M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.04
Mn - 1.50
Si - 1.00
P - 0.04
S - 0.03
Cr 24.00 27.00
Ni 4.50 6.50
Mo 2.90 3.90
Cu 1.50 2.50
N 0.10 0.25

SA-479 S32550 - Detail

Specification for Stainless Steel Bars and Shapes for Use in Boilers and Other Pressure Vessels

Mechanical properties of grade SA-479 S32550 SA-479/SA-479M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
189 (≥) 646 (≥) 43 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade SA-479 S32550 SA-479/SA-479M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
786 (≥) 366 (≥) 12 23 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
548 483 646