SB-163 N08800 Stainless Steels to SB-163

SB-163 N08800 - Specification & Application

  • SB-163 - Specification for Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tubes

Specification for Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tubes

Chemical composition(wt.%) of SB-163 N08800 grade: to SB-163

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Mn - 1.50
Si - 1.00
P - 0.045
S - 0.015
Cr 19.00 23.00
Ni 30.00 35.00
Mo - -
Ti 0.15 0.60
Al 0.15 0.60

SB-163 N08800 - Detail

Specification for Seamless Nickel and Nickel Alloy Condenser and Heat-Exchanger Tubes

Mechanical properties of grade SB-163 N08800 SB-163

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
573 (≥) 674 (≥) 12 23 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade SB-163 N08800 SB-163

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
365 (≥) 611 (≥) 24 24 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 232
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
384 729 541

Equivalent Products