ЖC3 Stainless Steels

ЖC3 - Specification & Application

Russia TY standard grades and chemical compositions of the high temperature alloy castings

Chemical composition(wt.%) of ЖC3 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.11 0.16
Cr 14.00 18.00
Al 1.60 2.20
Mo 3.00 4.50
Ti 1.60 2.30
Co - -
W 4.50 6.50
Ni - remaining
Nb - -
Fe - 8.00
B - 0.02
Ce - -
V - 0.30
Zr - -
Mn - 0.60
Si - 0.60
S - 0.009
P - 0.015

ЖC3 - Detail

Russia TY standard grades and chemical compositions of the high temperature alloy castings

Mechanical properties of grade ЖC3

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
313 (≥) 424 (≥) 24 11 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade ЖC3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
731 (≥) 657 (≥) 34 41 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
473 819 367

Equivalent Products

We can customize the production of ЖC3 grade, contact us for the best solution.