04X14T3P1Φ Stainless Steels

04X14T3P1Φ - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 04X14T3P1Φ grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.02 0.06
Si - 0.50
Mn - 0.50
P - 0.030
S - 0.020
Cr 13.00 16.00
Ni - 0.50
Mo - 0.30
Co 5.80 7.00
Ti 0.30 0.60
Al 0.10 0.25
V 0.05 0.25
Nb 0.05 0.15
Ca 0.03 0.20
Zr 0.02 0.15
B - 0.008

04X14T3P1Φ - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 04X14T3P1Φ

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
275 (≥) 411 (≥) 34 33 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade 04X14T3P1Φ

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
129 (≥) 735 (≥) 23 44 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
557 497 566

Equivalent Grade

Equivalent Products

We can customize the production of 04X14T3P1Φ grade, contact us for the best solution.