06X14H6Д2MБT Stainless Steels

06X14H6Д2MБT - Specification & Application

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(wt.%) of 06X14H6Д2MБT grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.08
Si - 0.70
Mn - 1.00
P - 0.020
S - 0.018
Cr 13.50 14.50
Ni 5.50 6.00
Mo 1.40 1.70
Cu 2.00 2.50

06X14H6Д2MБT - Detail

Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Mechanical properties of grade 06X14H6Д2MБT

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
945 (≥) 265 (≥) 11 31 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 334

Physical properties of grade 06X14H6Д2MБT

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
825 (≥) 297 (≥) 34 44 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 211
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
436 866 491

Equivalent Grade

Equivalent Products

We can customize the production of 06X14H6Д2MБT grade, contact us for the best solution.